Pitting, crevice and galvanic corrosion of REX stainless-steel/CoCr orthopedic implant material

Paper ID Volume ID Publish Year Pages File Format Full-Text
13353 851 2002 7 PDF Available
Title
Pitting, crevice and galvanic corrosion of REX stainless-steel/CoCr orthopedic implant material
Abstract

The corrosion behavior of surgical implant CoCr alloy and REX 734 steel has been investigated. The pitting or crevice corrosion potentials have been determined to reach values as high as 500 mV vs. SCE for CoCr and 450 mV vs. SCE for REX 734. The galvanic corrosion behavior of CoCr/REX 734 couples has been evaluated with various electrochemical techniques. The measurement of the corrosion current of the galvanic couple as well as its prediction by applying mixed potential theories on measured potentiodynamic polarization curves revealed low galvanic currents in the range of nanoamperes.

Keywords
Electrochemistry; Pitting; Crevice and galvanic corrosion; Stainless steels; CoCr alloy; Orthopedic prostheses
First Page Preview
Pitting, crevice and galvanic corrosion of REX stainless-steel/CoCr orthopedic implant material
Get Full-Text Now
Don't Miss Today's Special Offer
Price was $35.95
You save - $31
Price after discount Only $4.95
100% Money Back Guarantee
Full-text PDF Download
Online Support
Any Questions? feel free to contact us
Publisher
Database: Elsevier - ScienceDirect
Journal: Biomaterials - Volume 23, Issue 16, August 2002, Pages 3479–3485
Authors
, , , , ,
Subjects
Physical Sciences and Engineering Chemical Engineering Bioengineering
Get Full-Text Now
Don't Miss Today's Special Offer
Price was $35.95
You save - $31
Price after discount Only $4.95
100% Money Back Guarantee
Full-text PDF Download
Online Support
Any Questions? feel free to contact us